Xylene

Petroleum xylene is a mixture of three isomers (ortho-, meta-, para-) and ethylbenzene, in demand for polymers, plasticizers, and coatings. This material examines GOST 9410-78 grades, physicochemical parameters, selection criteria for specific processes, and practical aspects of storage, transportation, and customs classification. Special attention is given to isomer differences and laboratory control methods.
  • CAS №:
Availability: In Stock

Petroleum Xylene: Technical Overview for Industrial Applications

Xylene (dimethylbenzene, C8H10) is an aromatic hydrocarbon existing as three isomers: ortho-, meta-, and para-xylene. In industrial practice, petroleum xylene is produced by catalytic reforming or pyrolysis of petroleum fractions, as well as by toluene disproportionation. The technical product is a mixture of three isomers and ethylbenzene. Its primary role is to provide the feedstock base for terephthalic acid (PET), phthalic anhydride, and isophthalic acid production, and to serve as a solvent for coatings and a high-octane fuel additive.

Chemical Identification

Xylenes are identified by CAS 1330-20-7 (mixed isomers), empirical formula C8H10, relative molecular mass 106.17. In international trade, they are classified under HS heading 2902: o-xylene 2902 41 000 0, m-xylene 2902 42 000 0, p-xylene 2902 43 000 0, and mixed xylene isomers 2902 44 000 0. Synonyms include dimethylbenzene, xylol, and petroleum xylene. Xylene is assigned to hazard class 3 for health effects (moderately hazardous substance).

Physicochemical Properties

Xylene is a colorless transparent liquid with a characteristic odor. Density at 20 degrees Celsius is 0.862-0.868 g/cm3 for grade A and 0.860-0.870 g/cm3 for grade B under GOST 9410-78. Initial boiling point is not below 137.5 degrees Celsius for grade A and 137.0 degrees Celsius for grade B. Boiling points of isomers are: o-xylene 144.1 degrees Celsius, m-xylene 139.1 degrees Celsius, p-xylene 138.5 degrees Celsius. Flash point in a closed cup is not below 23 degrees Celsius. Explosive limits in air are 1.0 percent (lower) and 7.1 percent (upper) by volume. Solubility in water is very low; xylene is miscible with most organic solvents.

Technical Grades and Supply Forms

Petroleum xylene is produced under GOST 9410-78 in two grades: A (OKP 24 1451 0110) and B (OKP 24 1451 0140). Grade A is intended for isomer separation and solvent use; grade B primarily as a solvent. Aromatic hydrocarbon content for grade A is at least 99.6 percent; for grade B it is not regulated. The product is supplied in rail and road tank cars, steel drums, intermediate bulk containers, and tank containers. Typical B2B shipments start from one tonne.

Regulatory Framework

In the EAEU region, quality is governed by GOST 9410-78. The standard covers petroleum xylene, a mixture of three xylene isomers and ethylbenzene obtained by aromatization of petroleum fractions, intended for isomer separation and use as a solvent for paints and varnishes. Packaging, marking, transportation, and storage are regulated by GOST 1510. For customs purposes, the explanatory notes to HS heading 2902 apply.

Mechanism of Action and Functional Role

In chemical synthesis, xylene isomers play distinct roles. Para-xylene is oxidized to terephthalic acid, which is further used for polyethylene terephthalate (PET) and polybutylene terephthalate (PBT). Ortho-xylene is oxidized to phthalic anhydride, used in plasticizer production. Meta-xylene is oxidized to isophthalic acid, used in unsaturated polyester resins. As a solvent, xylene physically dissolves alkyd, epoxy, and polyurethane resins by penetrating between polymer macromolecules and disrupting intermolecular bonds. After application, xylene evaporates at a controlled rate without chemically reacting with the film former.

Applications by Industry

The petrochemical industry consumes the largest share of xylene for terephthalic acid (via para-xylene) and subsequently PET, as well as phthalic anhydride (via ortho-xylene) and isophthalic acid (via meta-xylene). The coatings industry uses xylene as a solvent for alkyd, epoxy, and polyurethane materials. The fuel sector applies xylene as a high-octane additive to motor fuels. In pharmaceutical and dye production, xylene serves as a starting compound and solvent. Xylene is also used in printing and pesticide production.

Comparison with Alternative Materials

Compared with benzene, xylene is less toxic (hazard class 3 versus class 2 for benzene) and has a higher boiling point, reducing volatility. Compared with toluene, xylene offers somewhat lower solvency but is less toxic in several respects and provides slower evaporation, which may be preferable in certain formulations. Compared with aliphatic solvents such as naphtha or white spirit, xylene provides higher solvency for resins but requires stricter ventilation control.

Typical Processing Errors

  • Using xylene in unventilated enclosed spaces without respiratory and skin protection.
  • Mixing xylene with oxidizers such as nitric acid or peroxides, which may cause an exothermic reaction.
  • Storing drums under direct sunlight or near heat sources, leading to pressure buildup and leaks.
  • Applying xylene to waterborne paints, causing dispersion coagulation.
  • Using product past its shelf life without prior laboratory verification of main substance content and impurities.
  • Working with xylene without equipment grounding, creating a risk of static electricity accumulation.

Quality Control and Laboratory Methods

Incoming inspection of petroleum xylene includes determination of appearance and color (GOST 2706.1-74), density at 20 degrees Celsius (hydrometer or pycnometer under GOST 3900-85), distillation limits (GOST 2706.13-74), aromatic hydrocarbon content (GOST 2706.2-74), sulfuric acid color (GOST 2706.3-74), hydrogen sulfide and mercaptan content, aqueous extract reaction (GOST 2706.7-74), evaporability (GOST 2706.8-74), and flash point (GOST 6356-75). Ethylbenzene and non-aromatic hydrocarbon content are regulated separately.

Storage and Transportation Conditions

Xylene is a flammable liquid. The closed-cup flash point is not below 23 degrees Celsius, corresponding to hazard class 3 under GOST 12.1.007. Storage is in sealed containers in ventilated warehouses, protected from direct sunlight and kept away from oxidizers and ignition sources. In storage and application areas, open flames and spark-producing tools are prohibited. The guaranteed shelf life of xylene under GOST 9410-78 is one year from the date of manufacture. Transportation is possible by all modes of transport in compliance with dangerous goods regulations: UN 1307, class 3, packing group III.

Finding Analogues and Interchangeability

When selecting an analogue for xylene, the key criteria are isomer composition, solvency (aniline point), flash point, toxicity, and compatibility with the formulation. Toluene can partially replace xylene in coating formulations, but this alters evaporation rate. For terephthalic acid synthesis, high-purity para-xylene or mixtures enriched in the para-isomer are required. Direct substitution without preliminary testing is not recommended.

Supply Scheme

For industrial buyers, petroleum xylene is available worldwide through the apptrade.ru platform. Shipments can be organized from producing regions across different continents, with logistics and customs support adapted to the destination market. International sourcing allows buyers to balance cost and lead time depending on batch size and logistical distance.

Logistics and Customs Clearance

Xylene is transported by sea, rail, and road. For large batches, sea tank containers or dedicated tankers are economically viable; for medium and small volumes, intermediate bulk containers and steel drums are used. When imported into the EAEU, products are classified under HS heading 2902, requiring accurate description of isomer composition. The portal customs broker prepares declarations, confirms classification codes, and manages non-tariff regulation procedures where applicable.

FAQ

What is the difference between xylene and toluene?

Xylene (C8H10) contains two methyl groups and exists as three isomers, with a boiling point of 137-144 degrees Celsius. Toluene (C7H8) contains one methyl group, is more volatile (boiling point 110.6 degrees Celsius), and has somewhat higher solvency.

Can xylene be used to thin waterborne paints?

No. Xylene is incompatible with aqueous systems and may cause dispersion coagulation. It is intended for solvent-borne materials.

What hazard class is assigned to xylene?

Petroleum xylene is hazard class 3 for health effects (moderately hazardous). For transport, it is class 3 flammable liquid, UN 1307.

How long can xylene be stored?

The guaranteed shelf life of xylene under GOST 9410-78 is one year from the date of manufacture. After expiry, the product must undergo laboratory testing before use.

Is special packaging required for transportation?

Yes. For class 3 dangerous goods, packaging must withstand internal pressure and comply with ADR requirements. Hazard labels are applied in accordance with GOST 19433.

What is the difference between grades A and B under GOST 9410-78?

Grade A is intended for isomer separation and solvent use and contains at least 99.6 percent aromatic hydrocarbons. Grade B is used primarily as a solvent, and its aromatic hydrocarbon content is not regulated.

How do xylene isomers differ in application?

Para-xylene is feedstock for terephthalic acid and PET. Ortho-xylene is used for phthalic anhydride and plasticizers. Meta-xylene is used for isophthalic acid and unsaturated polyester resins.

Conclusion

Petroleum xylene remains a foundational petrochemical intermediate and industrial solvent due to its predictable quality, established regulatory framework, and availability. For B2B buyers, critical factors include batch-to-batch isomer consistency, correct customs classification, and compliance with dangerous goods transport rules. The apptrade.ru portal organizes the full supply cycle, from grade selection for a specific process to customs clearance and delivery to the manufacturing site.

Contact Us

For procurement inquiries, technical documentation, and logistics coordination, contact the apptrade.ru team at info@apptrade.ru.