Sulfuric acid (H2SO4) is a heavy oily colorless and odorless liquid miscible with water in all proportions with the release of significant heat. Industrially, it is produced by the contact process through catalytic oxidation of sulfur dioxide to sulfur trioxide followed by absorption in water or sulfuric acid. Global sulfuric acid production exceeds 250 million tonnes per year, placing it among the largest-volume chemical products.
For procurement teams, sulfuric acid matters primarily as a reagent for phosphate and nitrogen fertilizer production, as well as a process agent in metallurgy, oil refining and chemical synthesis. GOST 2184-2013 provides for several product types differing in monohydrate concentration and impurity content, enabling selection of the grade for a specific process.
The key feature of sulfuric acid that determines the entire handling chain is the combination of strong acidic and dehydrating properties with high corrosiveness and the ability to cause chemical burns. The product is classified as a class 8 hazardous good (corrosive substances), UN number 1830, requiring specialized packaging, trained personnel and strict compliance with transport regulations.
In the Russian regulatory system, the primary document for technical sulfuric acid is GOST 2184-2013, which covers contact (improved and technical), oleum (improved and technical) and regenerated acid. The standard establishes requirements for physical and chemical parameters, acceptance rules and analytical methods. The supplier confirms batch conformity to GOST 2184-2013 and provides a certificate of quality with actual values for each parameter.
For the processor and logistics specialist, the high density and viscosity of concentrated acid, which complicate pumping at low temperatures, are critical, as is the ability of dilute acid to actively dissolve metals. Concentrated acid passivates many metals through the formation of a dense oxide film, while dilute acid requires acid-resistant materials.
The purest product type with a monohydrate mass fraction of 92.5-94.0 percent and minimal content of iron, nitrogen compounds and calcination residue. Used in productions where reagent purity critically affects target product quality, including caprolactam, titanium dioxide and pharmaceutical substances.
Produced in two grades. Grade 1 contains not more than 0.02 percent iron and not more than 0.05 percent calcination residue; grade 2 allows wider impurity limits. Used in fertilizer production, metal pickling and other processes not requiring high purity.
A solution of sulfur trioxide in sulfuric acid with a free sulfur anhydride mass fraction of at least 19-24 percent. Used to produce highly concentrated sulfuric acid, in sulfonation processes and as a dehydrating agent. Improved oleum intended for caprolactam production is supplied, at consumer request, with a free anhydride mass fraction of at least 19 percent.
Obtained by regenerating spent acid and contains a wider range of impurities, including organic compounds and nitro compounds. Used in less demanding processes, such as certain fertilizer productions and neutralization.
Supply is in bulk in specialized rail and road tank cars, IBCs and tank containers. Glass carboys and polymer canisters are used for small batches.
For imported batches, the specification is based on manufacturer standards and harmonized ISO and ASTM methods. The batch specification is confirmed by the manufacturer certificate of quality and the results of incoming laboratory control by the recipient.
Sulfuric acid is one of the most active inorganic acids. It dissociates in aqueous solutions to form hydrogen and sulfate ions, providing a highly acidic environment. In the concentrated state, the acid exhibits strong dehydrating properties, removing water from organic compounds and causing charring. The oxidizing properties of concentrated acid allow it to react with metals after hydrogen in the activity series, although the reaction often proceeds with the release of sulfur dioxide rather than hydrogen.
In fertilizer production, sulfuric acid reacts with phosphate raw materials to form phosphoric acid and calcium sulfate, and with ammonia to form ammonium sulfate. In metallurgy, the acid is used for metal pickling, removing oxides and scale from the surface of steel and non-ferrous metals. In oil refining, it is used to treat petroleum products to remove unsaturated hydrocarbons and sulfur compounds. In chemical synthesis, the acid serves as a catalyst, sulfonating agent and dehydrating agent.
For the B2B buyer, it is important to understand that acid concentration and impurity profile directly affect reaction rates, target product yield and corrosive attack on equipment. Iron and nitrogen compound impurities can catalyze side reactions and contaminate the final product, so control under GOST 2184-2013 is a mandatory incoming inspection step.
Dominant consumption direction. Sulfuric acid is used to decompose phosphate raw materials (apatite, phosphorite) to produce phosphoric acid and single superphosphate, as well as to produce ammonium sulfate by reaction with ammonia. This segment accounts for a significant share of global acid consumption.
Pickling of steel and non-ferrous metals to remove scale and oxides before rolling, drawing or coating. The acid is also used in metal refining and electrolysis processes, including copper, zinc and nickel production.
Treatment of petroleum products to remove unsaturated hydrocarbons and sulfur compounds, alkylation of isobutane with olefins, production of caprolactam, titanium dioxide and various organic dyes.
Production of mineral salts and acids, explosives, artificial fibers, detergents and pharmaceutical substances. The acid is also used as a dehydrating and drying agent in laboratory and industrial practice.
Production of battery electrolyte, water and wastewater treatment, metal surface treatment before painting, as well as in the textile and leather industries.
Compared with hydrochloric acid, sulfuric acid provides a higher boiling point and is less volatile, allowing processes to be conducted at elevated temperatures without significant reagent loss. Compared with nitric acid, sulfuric acid is a stronger dehydrating agent and is more often used for drying gases and organic liquids. Compared with phosphoric acid, sulfuric acid has higher acidity and oxidizing ability but is inferior in its ability to form soluble salts with certain metals.
In fertilizer production, sulfuric acid competes with nitric acid in phosphate raw material decomposition processes, but the choice is determined by raw material availability and final product requirements. In metallurgy, sulfuric acid is often replaced by hydrochloric acid for pickling stainless steels, since hydrochloric acid is less prone to surface passivation.
For chemical synthesis, sulfuric acid remains an irreplaceable sulfonating and dehydrating agent in large-tonnage processes, reinforcing its position as a base product of inorganic chemistry.
The specification for sulfuric acid must include the product type (contact improved, technical, oleum, regenerated), grade, monohydrate mass fraction, limit values for iron, calcination residue and nitrogen compounds, as well as packaging and transport requirements.
The supplier confirms batch-to-batch quality consistency, a valid safety data sheet under GOST 30333-2022, readiness to provide transport authorized for class 8 dangerous goods and to organize loading in compliance with safety measures. For imported batches, it is important to verify that marking and actual parameters match, since grade designations may differ.
Incoming inspection of sulfuric acid includes determination of the monohydrate mass fraction (titration), iron mass fraction (photometric or atomic absorption), calcination residue (gravimetric), nitrogen oxides and nitro compounds, as well as transparency and color for improved grades. Sampling is performed in acid-resistant containers with observance of safety measures; the combined sample is analyzed in the plant laboratory.
When changing supplier or batch, a control run of the target product is recommended to confirm compatibility with the process. For oleum, the free sulfur anhydride mass fraction is additionally controlled.
Sulfuric acid is classified as a class 8 dangerous good (corrosive substances), subclass 8.1, UN number 1830, and requires specialized steel tank cars, IBCs and tank containers. Storage is carried out in above-ground or underground tanks made of acid-resistant materials, equipped with breather valves, level and temperature control systems, and spill neutralization equipment.
Transportation is carried out in rail and road tank cars, tank containers and IBCs. According to industry sources, the share of tank containers in rail transport of sulfuric acid reached 41 percent in 2024, driven by their increased safety and suitability for multimodal transport. Sea transport uses specialized tank containers and vessels complying with IMDG requirements.
There is no direct analogue of sulfuric acid as a sulfonating and dehydrating agent in large-tonnage processes. In some applications, such as certain neutralization processes, sulfuric acid can be replaced by hydrochloric or nitric acid, but this changes the reaction product composition and requires process revision. In fertilizer production, replacement of sulfuric acid with nitric acid is possible only with a change in the final product type.
When changing supplier, a product of the same type and grade with similar monohydrate and impurity parameters is selected. The replacement decision is based on laboratory testing and, for critical processes, pilot-scale verification.
Domestic supply is provided by non-ferrous metallurgy enterprises and chemical complexes where sulfuric acid is produced as a primary or by-product. Products are supplied to the domestic market and for export. Shipment is carried out by rail, through ports and pipeline systems.
China is the largest producer and consumer of sulfuric acid. In 2026, China imposed a ban on sulfuric acid exports, creating tension in the global market. Russian suppliers retain the ability to export, but logistics require consideration of regulatory restrictions. Other global producers are located in the Middle East, Southeast Asia and Europe. Suppliers from these regions are engaged when required, taking into account logistical and regulatory factors and the availability of specialized transport for dangerous goods.
Bulk transport of sulfuric acid is carried out in specialized rail tank cars, tank containers and road tankers. Customs clearance includes classification under HS code 2807000000, preparation of a safety data sheet under GOST 30333-2022, conformity declaration and compliance with dangerous goods labeling requirements. For imported batches, permits and compliance of packaging with international requirements are additionally verified. The portal provides customs broker services and supports all clearance stages.
The main risks are associated with chemical burns to skin and eyes, corrosive attack on equipment and release of toxic vapors on contact with organic materials. Sulfuric acid causes severe burns; in case of skin contact, the affected area must be immediately flushed with large amounts of water and medical attention sought. Work is performed in ventilated rooms with acid-resistant gloves, protective goggles and protective clothing.
In case of a spill, the area is cordoned off, the spill is neutralized with alkaline solutions (lime, soda), then collected and disposed of in accordance with requirements. Discharge of acid into sewers and water bodies is not permitted. Process regulations provide level and temperature interlocks, emergency relief to a safe vessel, and periodic monitoring of vapor concentration in the working area air.
Improved acid has a narrower monohydrate concentration range (92.5-94.0 percent) and reduced impurity content, especially iron and calcination residue. Technical acid of grades 1 and 2 allows wider impurity limits and is used in less demanding processes.
Oleum is a solution of sulfur trioxide in sulfuric acid. It is used to produce highly concentrated sulfuric acid, in sulfonation processes and as a dehydrating agent. Improved oleum intended for caprolactam production is supplied with a free anhydride mass fraction of at least 19 percent.
Steel tanks are used for concentrated acid, and acid-resistant or rubber-lined tanks for dilute acid. Transportation is carried out in specialized tank cars, IBCs and tank containers.
Import requires a contract, invoice, packing list, safety data sheet under GOST 30333-2022 in Russian, manufacturer certificate of quality, transport documents and a declaration of conformity. For dangerous goods, transport permits and compliance with carriage rules are additionally confirmed.
The monohydrate mass fraction, density, iron content and calcination residue are determined. For improved acid, transparency and color are additionally controlled. Sampling is performed in acid-resistant containers with observance of safety measures.
Sulfuric acid remains an indispensable large-tonnage inorganic product, enabling fertilizer production, non-ferrous metallurgy, oil refining and chemical synthesis. GOST 2184-2013 establishes acid types and grades differing in concentration and impurity content, enabling selection of the product for a specific process. For procurement teams, the practical task reduces to correct selection of acid type and grade, confirmation of batch conformity to the standard, and organization of supplies in compliance with dangerous goods transport rules and safety measures.
For procurement inquiries and supply chain organization, contact the portal team at info@apptrade.ru.