Agricultural urea (grade B) is the amide of carbamic acid, produced by synthesis from ammonia and carbon dioxide. In the agro-industrial complex, urea occupies a central position as the most concentrated solid nitrogen fertilizer. Its primary function is to supply plants with nitrogen in amide form, which gradually transforms in the soil into forms available to the root system, providing prolonged nutrition throughout the growing season. Grade B is intended for crop production, livestock farming, and retail sale, making it a versatile product for agricultural producers.
Urea is identified by CAS 57-13-6, empirical formula CO(NH2)2, relative molecular mass 60.06. In international trade, it is classified under HS heading 3102 10 as urea containing more than 45 percent by mass of nitrogen on the dry anhydrous product. Synonyms include carbamide and carbonyldiamide. Grade B is not classified as dangerous goods for transport and is fire- and explosion-safe under normal conditions. When heated above the melting point, urea tends to form biuret, the content of which in the agricultural grade is strictly regulated.
Urea grade B consists of white or slightly colored granules or crystals. The nitrogen mass fraction calculated on dry substance is at least 46.2 percent. The biuret mass fraction must not exceed 1.4 percent for all grades of grade B for crop production, which is important for preventing plant suppression. Water mass fraction: hygroscopic not more than 0.3 percent, total not more than 0.5-0.6 percent depending on the grade. Granulometric composition: the mass fraction of granules sized 1 to 4 mm is at least 94 percent, granules below 1 mm not more than 3-5 percent, and residue on a 6 mm sieve is absent. Granule static strength is at least 3 N per granule, and flowability is 100 percent. Density at 25 degrees Celsius is 1330 kg/m3, bulk density of the granular product is 687-736 kg/m3. Melting point is 132.7 degrees Celsius. Urea is readily soluble in water: at 20 degrees Celsius, 51.8 g dissolves in 100 g of water; at 60 degrees Celsius, 71.7 g.
Under GOST 2081-2010, urea is produced in two grades: A for industry and B for crop production, livestock farming, and retail sale. Within grade B for crop production, highest, first, and second grades are distinguished, differing in biuret content and granulometry. The product is supplied in bulk in rail cars and road transport, in polypropylene bags of 50 kg, and in big bags of 800 and 1000 kg capacity. Typical agricultural bulk shipments start from one tonne; for large agroholdings, from 20 tonnes.
In the EAEU region, quality of agricultural urea is governed by GOST 2081-2010 Urea. Specifications. The standard sets requirements for physicochemical indicators of grade B, packaging, marking, transportation, and storage. The product, as a mineral fertilizer, is subject to conformity declaration under the EAEU technical regulation on requirements for mineral fertilizers, which sets radiation and chemical safety norms. For customs purposes, the explanatory notes to HS heading 3102 10 apply.
In the soil, urea is hydrolyzed by the enzyme urease to ammonia and carbon dioxide. Ammonia reacts with water to form ammonium hydroxide, which is then nitrified by microorganisms to nitrates available to plants. The amide form of nitrogen provides a more gradual release compared with nitrate forms, reducing leaching losses. Foliar feeding with urea solution is effective due to the low biuret content and the ability of leaves to absorb amide nitrogen. In livestock farming, urea is used as a source of non-protein nitrogen for ruminants, where rumen microflora synthesizes protein from it.
Crop production consumes the largest share of urea grade B. The product is used as a basal fertilizer for all agricultural crops on all soil types, for pre-sowing application, and for root and foliar top dressing. Urea is especially valued in rice cultivation, for foliar feeding of vegetables and fruit crops, and for late top dressing of wheat to increase protein and gluten content in grain. Application rates range from 25 to 500 kg/ha per year depending on the crop, planned yield, and soil agrochemical parameters. In livestock farming, urea is used as a feed additive for ruminants to compensate for protein deficiency. In industry, grade A is used for resin and adhesive production, but grade B is supplied for agricultural procurement.
Compared with ammonium nitrate, urea contains a higher nitrogen concentration (46.2 percent versus 35 percent), reducing storage and transport costs per unit of active ingredient. Compared with ammonium sulfate, urea provides higher nitrogen content and does not acidify the soil as strongly. Compared with urea-ammonium nitrate solution, urea is a solid product that simplifies storage and application, but UAN provides more uniform field distribution. The choice between these forms is determined by application technology and the requirements of the specific crop.
Incoming inspection of urea grade B includes determination of appearance and color, nitrogen mass fraction calculated on dry substance, biuret mass fraction, water mass fraction (hygroscopic and total), granulometric composition, granule static strength, and flowability. Nitrogen content is determined by ammonia distillation after urea decomposition with sulfuric acid. Biuret content is determined by photometric method. Test methods are governed by GOST 2081-2010 and relevant standards for mineral fertilizer analysis.
Urea must be stored in closed, well-ventilated warehouses protecting the product from atmospheric precipitation. When storing in bulk, mixing urea with other fertilizers should be avoided. The guaranteed shelf life is 6 months from the date of manufacture; the service life is unlimited. Urea is not classified as dangerous goods for transport, simplifying logistics. Transportation is carried out by all modes of transport in accordance with cargo transport rules. For sea shipments, bulk transport in bulkers or big bags in containers is used.
When selecting an analogue for agricultural urea, the key criteria are nitrogen content, biuret content, granulometric composition, and application. For biuret-sensitive crops, urea of the highest grade with a biuret content not exceeding 0.6 percent is preferable. For basal application to cereals, replacement with ammonium nitrate or urea-ammonium nitrate solution is possible with dosage adjustment for nitrogen. For foliar feeding, replacement with other nitrogen forms requires revision of the solution concentration. Direct substitution without consideration of agronomic requirements is not recommended.
For agricultural producers and industrial buyers, agricultural urea is available worldwide through the apptrade.ru platform. Shipments can be organized from producing regions across different continents, with logistics and customs support adapted to the destination market. International sourcing allows buyers to balance cost and lead time depending on batch size and logistical distance, especially for bulk sea shipments.
Urea is transported by sea, rail, and road. For large batches, bulk transport in sea bulkers or mineral carriers is economically viable; for medium and small volumes, big bags and sacks are used. When imported into the EAEU, products are classified under HS heading 3102 10. As urea is not dangerous goods, special dangerous goods packaging and marking requirements do not apply; however, phytosanitary and sanitary norms must be observed. The portal customs broker prepares declarations, confirms classification codes, and manages non-tariff regulation procedures.
Urea grade A is intended for industry, including the production of resins, adhesives, and feed additives for animals. Grade B is intended for crop production, livestock farming, and retail sale. For agricultural procurement for crops, grade B is supplied, having passed the appropriate biuret and granulometry control.
Yes, urea is widely used for foliar feeding of vegetables, fruit crops, and late top dressing of wheat. For these purposes, urea with low biuret content (highest grade) is recommended, and solutions should be prepared at a concentration that does not cause leaf burns.
No, urea is not classified as dangerous goods for transport. It is fire- and explosion-safe under normal conditions, does not require special permits or dangerous goods marking, simplifying logistics and storage.
The nitrogen mass fraction calculated on dry substance for urea grade B is at least 46.2 percent. This is the most concentrated solid nitrogen fertilizer.
The guaranteed shelf life of urea is 6 months from the date of manufacture under storage conditions in closed, well-ventilated warehouses. The service life is unlimited, but after the guaranteed period, the product must undergo laboratory testing before use.
Urea can be mixed with superphosphate and potassium chloride on the day of sowing. Mixing with ammonium nitrate requires caution due to possible complex compound formation. Compatibility testing is recommended before preparing fertilizer blends.
Agricultural urea (grade B) remains a foundational nitrogen fertilizer for crop production and an important component of feed rations in livestock farming due to its high nitrogen concentration, availability, and established regulatory framework. For agro-industrial buyers, critical factors include batch-to-batch consistency, especially biuret content and granulometry, correct customs classification, and compliance with storage conditions to prevent caking. The apptrade.ru portal organizes the full supply cycle, from grade selection for a specific crop to customs clearance and delivery to the manufacturing site.
For procurement inquiries, technical documentation, and logistics coordination, contact the apptrade.ru team at info@apptrade.ru.