Vinyl chloride (chloroethene, ethenyl chloride, monochloroethylene) is a chlorinated unsaturated hydrocarbon produced industrially by direct chlorination of ethylene followed by pyrolysis of ethylene dichloride or by oxychlorination of ethylene. In industrial practice, vinyl chloride occupies a central position as the monomer for large-scale production of polyvinyl chloride (PVC) and its copolymers. Its primary function is to provide the feedstock base for rigid and plasticized PVC used in construction, piping, cable insulation, window profiles, flooring, and medical devices. Virtually the entire global volume of vinyl chloride is consumed for PVC synthesis.
Vinyl chloride is identified by CAS 75-01-4, empirical formula C2H3Cl, structural formula CH2=CHCl, relative molecular mass 62.5. In international trade, it is classified under HS heading 2903 as halogenated derivatives of hydrocarbons. Synonyms include chloroethene, ethenyl chloride, monochloroethylene, and vinyl chloride monomer. The substance is assigned to hazard class 1 for health effects (extremely hazardous substance) and is classified as an IARC Group 1 carcinogen. At ambient conditions, vinyl chloride is a gas that is stored and transported in a liquefied state under pressure.
Vinyl chloride is a colorless gas with a mild sweetish odor that becomes a transparent liquid upon cooling or under pressure. Liquid phase density at 20 degrees Celsius is 0.9106 g/cm3. Boiling point is minus 13.8 degrees Celsius, melting point minus 153.8 degrees Celsius. Flash point is minus 78 degrees Celsius in a closed cup, autoignition temperature 472 degrees Celsius. Explosive limits in air are 3.6 percent (lower) and 33.0 percent (upper) by volume. Saturated vapor pressure at 20 degrees Celsius is about 337 kPa (about 2.5 atmospheres gauge). Vinyl chloride is poorly soluble in water (about 1.1 g/L at 25 degrees Celsius) and well soluble in ethanol and most organic solvents. It has a high tendency to spontaneous polymerization under the action of light, heat, air, and initiators, so the industrial product is stabilized with an inhibitor.
Vinyl chloride as a polymerization monomer is produced under manufacturer technical specifications, as no single state standard for the technical requirements of the monomer exists in the EAEU; current standards govern methods for determining residual monomer in polymers (in particular, GOST 25737-91). Technical specifications set requirements for product purity, impurity content (acetylene, ethylene dichloride, ethyl chloride, water), and inhibitor content. The product is supplied in a liquefied state under pressure in dedicated rail tank cars, tank containers, sea gas carriers, and cylinders. Typical bulk shipments start from one tonne.
No single technical regulation or state standard establishing technical requirements for commercial vinyl chloride as a monomer exists in the EAEU; a significant part of production is governed by manufacturer technical specifications. Methods for determining residual monomer in polymers are governed by GOST 25737-91. Vinyl chloride as dangerous goods is classified under GOST 19433 indicating hazard class 2.1 (flammable gases) and UN number 1086. For customs purposes, the explanatory notes to HS heading 2903 apply.
In polymerization processes, vinyl chloride undergoes chain reactions initiated thermally, photochemically, or by chemical initiators (peroxides, azo compounds). The double bond of the vinyl group opens, enabling the binding of monomer units into a polyvinyl chloride macromolecule. The chlorine atom imparts polarity, rigidity, flame resistance, and chemical resistance to the polymer. Depending on polymerization conditions (suspension, emulsion, bulk), PVC with different particle size, porosity, and molecular mass is obtained, which determines its processing into rigid or plasticized products.
Virtually the entire volume of vinyl chloride is consumed in the production of polyvinyl chloride, which is further processed into a wide range of products. In construction, PVC is used for window profiles, pipes, siding, flooring, and roofing membranes. In electrical engineering, it is used for cable insulation and wire sheaths. In the automotive industry, it is used for interior trim, seals, and under-hood parts. In medicine, it is used for tubing, blood bags, and disposable items. In packaging, it is used for films and bottles. Vinyl chloride copolymers with vinyl acetate are used in the coatings industry and artificial leather production.
Compared with ethylene and propylene, vinyl chloride provides polymers with a unique combination of flame resistance, chemical resistance, and mechanical strength due to the chlorine atom. Compared with fluoropolymers, PVC is significantly cheaper but inferior in heat resistance and chemical resistance to aggressive media. Compared with polyolefins, PVC offers higher rigidity and flame resistance but requires plasticizers and stabilizers to obtain flexible products and to be processed. In pipe and profile production, PVC competes with polyethylene and polypropylene, surpassing them in flame resistance but inferior in low-temperature impact strength.
Incoming inspection of vinyl chloride includes determination of appearance and color, density of the liquefied phase, main substance content by gas chromatography, impurity content (acetylene, ethylene dichloride, ethyl chloride, water), inhibitor content, and acidity. For critical applications, oxygen and peroxide content are controlled. Methods for determining residual monomer in polymers are governed by GOST 25737-91 and GOST ISO 6401-2021.
Vinyl chloride is stored in sealed pressure vessels designed for the working pressure of the liquefied gas, in ventilated premises protected from direct sunlight and heat sources. The storage temperature must not exceed the values specified in the technical specifications for the specific container type, typically not above plus 30-40 degrees Celsius. The guaranteed shelf life is typically 3 to 6 months depending on inhibitor content. Vinyl chloride is classified as dangerous goods: hazard class 2.1 (flammable gases), UN number 1086, packing group not applicable to gases; classification code 2111. Transportation is carried out in dedicated rail tank cars, tank containers, and sea gas carriers in accordance with dangerous goods regulations. Road transport follows ADR requirements; sea transport follows IMDG Code.
When selecting an analogue for vinyl chloride, the key criteria are product purity, inhibitor content, and impurity content. For PVC production, replacing vinyl chloride with other monomers (vinylidene chloride, vinyl acetate, acrylonitrile) alters the properties of the final polymer and requires revision of the entire formulation and technology. In copolymer production, vinyl chloride can be partially replaced by vinyl acetate or acrylates to impart flexibility and improve processability, but this changes the heat resistance and chemical resistance of the finished product. Direct substitution without preliminary testing is not recommended.
For industrial buyers, vinyl chloride is available worldwide through the apptrade.ru platform. Shipments can be organized from producing regions across different continents, with logistics and customs support adapted to the destination market. International sourcing allows buyers to balance cost and lead time depending on batch size and logistical distance.
Vinyl chloride is transported by sea, rail, and road in dedicated pressure vessels. For large batches, sea gas carriers or rail tank cars are economically viable; for medium and small volumes, tank containers and cylinders are used. When imported into the EAEU, products are classified under HS heading 2903. As vinyl chloride is class 2.1 dangerous goods, compliance with ADR and IMDG Code packaging, marking, and documentation requirements is mandatory. The portal customs broker prepares declarations, confirms classification codes, and manages non-tariff regulation procedures.
Vinyl chloride is a gas at ambient conditions with a boiling point of minus 13.8 degrees Celsius. For efficient transportation and storage, it is liquefied under pressure, which significantly reduces volume and allows the use of standard pressure vessels designed for flammable gases.
Vinyl chloride is hazard class 1 for health effects as an extremely hazardous substance and is classified as an IARC Group 1 carcinogen. For transport, it is classified as class 2.1 dangerous goods (flammable gases), UN number 1086.
Vinyl chloride tends to undergo spontaneous polymerization under the action of light, heat, atmospheric oxygen, and initiators. To prevent undesirable polymerization during storage and transportation, an inhibitor is introduced into the product; it is consumed first and requires periodic monitoring and replenishment.
The guaranteed shelf life of vinyl chloride is typically 3 to 6 months from the date of manufacture under proper temperature conditions and container tightness. After expiry or if the inhibitor content falls below the norm, the product must undergo laboratory testing before use.
Yes, because vinyl chloride is a liquefied gas under pressure and class 2.1 dangerous goods. Dedicated rail tank cars, tank containers, and sea gas carriers designed for working pressure and equipped with safety devices are used. Packaging must comply with ADR and IMDG Code requirements for flammable gases.
Vinyl chloride (C2H3Cl) is a gaseous monomer used for polymer synthesis. Polyvinyl chloride (PVC) is a solid polymer obtained by polymerizing vinyl chloride. Vinyl chloride is the starting feedstock; PVC is the final product.
Vinyl chloride remains a foundational monomer for polyvinyl chloride production, determining the properties of one of the largest-volume polymers in the world. For industrial buyers, critical factors include batch-to-batch consistency, especially inhibitor and impurity content, correct customs classification considering dangerous goods status, and compliance with pressurized storage conditions. The apptrade.ru portal organizes the full supply cycle, from grade selection for a specific process to customs clearance and delivery to the manufacturing site.
For procurement inquiries, technical documentation, and logistics coordination, contact the apptrade.ru team at info@apptrade.ru.