Zirconium Basic Carbonate | CAS 57219-64-4 | Catalyst Grade

White powder, soluble in hot concentrated acids but insoluble in water. Primarily used in catalyst production and manufacturing of other zirconium compounds.
  • CAS №: 57219-64-4
Availability: In Stock

Product Name: Zirconium Basic Carbonate
CAS No.: 57219-64-4
Molecular Formula: CH₂O₇Zr₂
Molecular Weight: 308.47
Appearance: White powder

Properties

  • Soluble in hot concentrated acids

  • Insoluble in water

Applications

  • Production of catalysts

  • Manufacturing of other zirconium compounds

Characteristics