Sodium Fluoride NaF CAS 7681-49-4

Sodium fluoride is an ionic compound with formula NaF. White crystals or powder, odorless. Soluble in water, slightly soluble in alcohol. Used as food fortifier, pharmaceutical intermediate, and dental caries preventive.
  • CAS №: 7681-49-4
Availability: In Stock

Sodium Fluoride (NaF) – Versatile Fluoride Compound for Industrial and Pharmaceutical Applications

Basic Information

  • CAS Number: 7681-49-4

  • Molecular Formula: NaF

  • Molecular Weight: 41.99 g/mol

  • Appearance: Colorless crystalline solid or white powder at room temperature, odorless.

  • Density: 2.25 g/cm³

  • Melting Point: 993°C

  • Boiling Point: 1695°C

  • Solubility: Soluble in water; slightly soluble in alcohol.

Overview
Sodium fluoride is an important ionic compound and a key fluoride product. It is widely used across multiple industries due to its unique chemical properties and high purity.

Applications

  • Dental care: Used as an active ingredient in toothpaste, mouthwashes, and dental treatments for caries prevention.

  • Food fortification: Added as a fluoride supplement in food products and drinking water to support dental health.

  • Pharmaceutical intermediates: Used in the synthesis of various pharmaceutical compounds and fluorine-containing drugs.

  • Metallurgy: Employed as a flux in aluminum and steel production.

  • Chemical industry: Raw material for the production of other fluoride compounds and specialized chemicals.

  • Glass and ceramics: Used in the manufacturing of specialty glasses and glazes.

Recommended Usage
In toothpaste and oral care products, typical concentrations range from 0.1% to 0.25% as fluoride ion. For water fluoridation, levels are adjusted to approximately 0.7–1.2 mg/L depending on local regulations.

Handling and Storage

  • Store in a cool, dry, well-ventilated area, away from acids (especially mineral acids).

  • Keep containers tightly sealed to prevent moisture absorption and contamination.

  • Use appropriate personal protective equipment (gloves, safety goggles, dust mask) when handling.

Safety
Sodium fluoride is toxic in high concentrations. Avoid inhalation of dust and contact with skin and eyes. In case of contact, rinse thoroughly with water. For detailed safety information, refer to the Safety Data Sheet (SDS).

Packaging
Available in 1 kg, 5 kg, 25 kg, and 50 kg bags/drums. Custom packaging upon request.

Quality Assurance
Each batch is tested for purity, fluoride content, and heavy metals to ensure compliance with regulatory standards.