Product Name: Matte Acrylic Cathodic Electrophoretic Lacquer GK-MEC2091
Description
GK-MEC2091 is a high-performance acrylic cathodic matte electrophoretic lacquer. It is manufactured from acrylic monomer modified by a special process.
Key features include:
High weather resistance
High corrosion resistance
High artificial sweat resistance
Hardness >5H
Applications
Widely used for decorative electroplating and metal surface protection for products such as:
Aluminum profiles
Locks
Lighting fixtures
Jewelry
Household appliances
Automotive and motorcycle accessories
Sanitary ware
Lighters
Luggage accessories
Luggage carts
Tools
Other light industrial products requiring film coating and decorative finishing
Packaging and Storage
20 kg/drum. Shelf life: 6 months at 15–25 °C