Product Name: 2,6-Butyl-Hydroxytoluene (BHT / Antioxidant)
Synonyms: Antioxidant 200, Antioxidant 264, Antioxidant T510, Antioxidant BHT
Description
Antioxidant BHT is an excellent general-purpose phenolic antioxidant.
As a feed antioxidant: It protects vitamins in feed and prevents oxidative loss of fats and proteins. It also has certain antibacterial properties. The maximum dosage is 150 g/ton.
Key Features:
Water-soluble antioxidant
Widely used in Russia and internationally
High antioxidant capacity
Good heat resistance
Good stability
No reaction with metal ions
No specific odor or color
Low cost (1/8–1/10 of the cost of BHA)
In China, still used as a primary antioxidant
Usage Note: Typically used in combination with BHA and citric acid or other organic acids as synergists.