Acrylic Cathodic Electrophoretic Lacquer GK-EC800 | Low-Temp Curing

High-performance cathodic acrylic low-temperature electrophoretic lacquer. Modified from acrylic monomer and low-temperature yellowing-resistant isocyanate. Excellent weather resistance, corrosion resistance, high hardness, low curing temperature. Wide application for decorative plating and metal surface protection.
  • CAS №:
Availability: In Stock

Product Name: Acrylic Cathodic Electrophoretic Lacquer GK-EC800

Description

This high-performance cathodic acrylic low-temperature electrophoretic lacquer GK-EC800 was developed by our company. It consists of an acrylic monomer and low-temperature yellowing-resistant isocyanate, modified using special technology.

Key features include:

  • Excellent weather resistance

  • Excellent corrosion resistance

  • Excellent artificial sweat resistance

  • High hardness

  • Low curing temperature

  • Easy to use

Applications

Widely used for decorative electroplating and metal surface protection for products such as:

  • Aluminum profiles

  • Locks

  • Lighting fixtures

  • Jewelry

  • Household appliances

  • Sanitary ware

  • Lighters

  • Luggage straps

  • Tools

  • Other light industrial products requiring corrosion protection

Packaging and Storage

20 kg/drum. Shelf life: 6 months at 15–25 °C