Product Name: Dispersed Tungsten Oxide Nanoparticles (Cesium Tungsten Oxide)
CAS No.: 13587-19-4
EINECS: 237-019-0
Molecular Formula: Cs₂O₄W
Active Content: 99.9%
Appearance: Blue powder
Applications
Primarily used as a thermal insulation agent for:
Architectural glass
Automotive films
Greenhouses
Related industries