Acrylates/C10-30 Alkyl Acrylate Crosspolymer (Carbomer)

Hydrophobically modified acrylic acid crosspolymer. Easily dispersible, low viscosity before neutralization, salt-tolerant, compatible with surfactants. Provides effective thickening, suspending, and stabilizing for skin care, clear gels, and shampoos.
  • CAS №:
Availability: In Stock

Acrylates/C10-30 Alkyl Acrylate Crosspolymer – Hydrophobically Modified Rheology Modifier for Cosmetics

Product Information

  • Product Name: GK CARBOMER FD2010

  • INCI Name: Acrylates/C10-30 Alkyl Acrylate Crosspolymer

  • Appearance: White to off-white powder

Overview
GK CARBOMER FD2010 is an easily dispersible, hydrophobically modified acrylic acid (ester) crosspolymer. It exhibits low dispersion viscosity prior to neutralization, allowing for convenient dispersion and processing during use. The polymer offers excellent salt tolerance, good surfactant compatibility, and can be used in formulations containing electrolytes. It provides efficient thickening, suspending, and stabilizing effects with high clarity, making it suitable for a wide range of personal care applications.

Key Properties

  • Low dispersion viscosity – easy to disperse and handle.

  • Good salt tolerance – stable in electrolyte-containing formulations.

  • Excellent surfactant compatibility – works well with anionic, nonionic, and amphoteric surfactants.

  • Effective thickening, suspending, and stabilizing – maintains product integrity and texture.

  • High transparency – ideal for clear gels and transparent formulations.

  • Hydrophobically modified – improves emulsion stability and sensory properties.

Applications

  • Skin care lotions and creams.

  • Clear skin care gels and hair styling gels.

  • Formulations containing ions and electrolytes.

  • Shampoos and conditioners.

  • Shower gels and body washes.

  • Sunscreens and after-sun products.

  • Makeup and color cosmetics.

Recommended Usage
Typical use levels: 0.1–1.0% by weight, depending on the desired viscosity and suspension properties. Optimize through formulation testing. Neutralize with alkaline agents (e.g., triethanolamine, sodium hydroxide, or aminomethyl propanol) to achieve thickening.

Handling and Storage

  • Store in a cool, dry place, away from moisture and direct sunlight.

  • Keep containers tightly sealed to prevent contamination.

  • Shelf life: typically 24 months under recommended storage conditions.

  • Use appropriate personal protective equipment (gloves, dust mask) when handling.

Packaging
Available in 25 kg bags, drums, or custom packaging upon request.

Quality Assurance
Each batch is tested for viscosity, pH, and performance properties to ensure consistent quality.